Gaby,
Sorry about your troubles. I've never run into it with through hole devices, but many times with SMT
types having been reflowed and often needing touched-up because of poor solder termination
solderability.
It sounds and looks (in x-section) like a smilar problem. The fine coil wires become detached under
thermal stress because of dissimilar expansion rates at the attachment "legs."
We solved some, not all, problems by changing a supplier once to improve solderability. In another
instance, we more carefully watched our profiles to do everything possible to avoid touch-up.
Good luck,
Earl Moon
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|