Has anyone ever heard of the "Woodrow test" for wave soldering? I believe
it involves running a component-less PCB with solder paste on it through the
wave solder to determine if the wave soldering process will cause the
top-side solder paste to reflow.
Can anyone give me more information about this test? Is it legit?
Thanks in advance.
Regards,
Richard Todd
Senior Engineer, Quality
SMT Machine Center
Panasonic Automotive Systems Company of America
Division of Panasonic Corporation of North America
776 Highway 74 South, Peachtree City, GA 30269
770-515-1087 Direct
770-486-2248 Fax
<mailto:[log in to unmask]> [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|