TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Douthit <[log in to unmask]>
Date:
Fri, 24 Oct 2003 15:08:20 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (63 lines)
True but plugging via holes with solder that are 0.5 mm from BGA
attachments is looking for trouble.

> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of David Douthit
> Sent: Friday, October 24, 2003 2:22 PM
> To: [log in to unmask]
> Subject: Re: [TN] Cleaning of via holes under components
>
>
> Brian,
>
> Well said (again!!)
>
> David A. Douthit
> Manager
> LoCan LLC
>
> Brian Ellis wrote:
>
> > I'm a proponent of plugging -- with solder! Not only does
> it stop the
> > contamination problem, but it is electrically and thermally
> desirable,
> > as well. However, it should be done from only one side
> unless you like
> > to see miniature Krakatoas.
> >
> > Brian
> >
> > Paul Baine wrote:
> > > Hello,
> > >
> > > One of our Design Engineers is designing a surface mount PCB
> > > assembly and would prefer not to have the via holes solder mask
> > > tented.  However, he is concerned that, if he does not call up
> > > solder mask tenting on his bare PCB drawing, foreign matter could
> > > find its way into a via hole and, if a component (e.g. an IC) was
> > > mounted over the via hole, the foreign matter might not
> be removed
> > > during the cleaning process.
> > >
> > > Has anyone had experience with this situation?  I would
> appreciate
> > > any help you could give me.
> > >
> > > Thanks very much in advance.
> > >
> > > Paul Baine
> > > Q.A. Manager
> > > C-Tech Ltd.
> > > Cornwall, Ontario, Canada

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2