Bev
We were able to remove entrapped glycols with long soak times at elevated
temps. (You might try repeated rinses.)
Of course, those tests were done on unpopulated boards.
Greg
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Wednesday, September 04, 2002 11:13 AM
To: [log in to unmask]
Subject: [TN] board contaminated with glycol
Technettters,
Say you had a populated, expensive circuit pack that had been contaminated
with ethylene glycol. Would you chuck it or clean it? I seem to recall
that before I entered the industry that there was a time when some type of
glycol was used on making printed circuit boards(?). The reason I mention
this, is if this were true, can glycols chemically bond at room temperature
to PCBs by more than hydrogen bonding, to the point where a water wash,
saponified or not, would not be able to remove the glycol. I am assuming
there are no standoff issues.
regards,
Bev Christian
Research in Motion
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|