TECHNET Archives

August 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Amol Kane (Asteelflash,US)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Amol Kane (Asteelflash,US)
Date:
Thu, 16 Aug 2012 08:40:54 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (71 lines)
Good point!.....I usually do square apertures on BGAs below 16 mil pad
size, but in this case I was afraid the joints would bridge if the ball
size increases due to voiding. I will have to try the square apertures
and see.

Thanks,
Amol

-----Original Message-----
From: Bush, Brien [mailto:[log in to unmask]] 
Sent: Thursday, August 16, 2012 11:32 AM
To: 'TechNet E-Mail Forum'; Amol Kane (Asteelflash,US)
Subject: RE: CSP BGAs

What type of paste are you using? We are processing a bga 1x.8 with a .5
pitch and .175 ball diameter. We are using a Kester lead free EM828
solder paste. We have the stencil Apertures cut square encompassing the
round pad. This allows for slightly more paste.
Hope this helps,
Brien

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
(Asteelflash,US)
Sent: Thursday, August 16, 2012 9:34 AM
To: [log in to unmask]
Subject: [TN] CSP BGAs

Dear Technetters,

We are going to be assembling some lead-free  1.6x0.8 mm micro BGAs with
0.5mm pitch and 0.17mm dia board pads. Anybody else have experience with
this small a package?....I am concerned that there won't be sufficient
flux in the tiny solder deposit to clean the oxides during reflow,
leading to graping and/or head in pillow situation. Do I need a dip
fluxer for the part to do a flux only attachment, or to augment the
amount of flux in the solderpaste-solder bump system? I am told I have
no time to do DOEs to determine stencil and reflow parameters, so I am
turning to technet for help.....any thoughts?





Regards,

Amol




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

WARNING: Export Control
This message, including any attachments, may contain technical data
within the definition of the International Traffic in Arms Regulations
(ITAR), and subject to the Export Control Laws of the U.S. Government.
Transfer of such information by any means to a foreign person, whether
in the United States or abroad, without proper export authorization or
other approval from the U.S. Department of State is prohibited.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2