In a message dated 02/10/2000 7:33:38 PM US Eastern Standard Time,
[log in to unmask] writes:

> Just got here a week ago one of the pcb aspects training consultants (i have
>  to do the real work, not lectures);
>  and this wise fellow recommenced :"brush and running tap water" .
>  I just gulped the suddenly dry air ; managed to scramble politically
correct
>  face (for some reason all eyes turned on me) ;
>  and uttered in classic English (opted out of classic Australian in this
>  public occasion): 'hmm, interesting' .

Yup, you have a career as a consultant.  Can't tell you the number of times I
have bit back the response "what idiot came up with this" and actually said
"I see".

>
>  But, yo' never know Faz , he maybe right, and i have a bigger fish to fry

Oh, hell no.  Only use a brush and running tap water if you are cleaning your
kids or your sneakers.  A brush and tap water is an excellent cleaning final
step if the goal is to produce scrap.

Doug Pauls

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2