TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
MIME-Version:
1.0
Sender:
Subject:
From:
Paul Gould <[log in to unmask]>
Date:
Thu, 23 Oct 1997 18:16:42 +0100
In-Reply-To:
X-To:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Paul Gould <[log in to unmask]>
Parts/Attachments:
text/plain (35 lines)
Rob van Pol wrote:-
>We have tried peelable solderresists but these are not 100 %
>resistant to the pressure during horizontal hot air levelling resulting
>in P/Sn particles on the Ni/Au contacts.
Hi Rob,

You are on the right track with peelable but maybe you are not coating
sufficient thickness. You really need a very thick coating of around 20
mils to be able to withstand the levelling air knives. I have no
experience of horizontal levelling but it must be much the same as
vertical to the peelable.

There are other types of water soluble non-peelable masks if you want to
get into more water washing. Fortunately, I have not needed to go that
far and so again have no experience of these. Stick with the peelable
method and try to make it work.

Good luck,
--
Paul Gould
[log in to unmask]
Isle of Wight,UK

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2