Hi Gaby,
Typically most of the manufacturer's (AVX, Murata, TDK, and Kemet to name
a few) have application notes and may be available on their websites.
Going back about 4 years ago, my evaluations (at a former employer) of
multilayer ceramic chip capacitors being wave soldered yielded the
following:
- orientation of the chip parallel with the wave (end terminations
simultaneously contact the wave)
- delta temperature from preheat to wave should be <120 C (the lower the
better but look at most vulnerable component for temperature limits at
preheat)
- 0805 {1206, 0805, 0603 were tested} cracked less than any other size
(after thermal cycling -- -40 to +100 C / most mfr's suggest not using
larger than 1206 but I would start with 0805 as long the values you need
are available in that size and of course if your CCA real estate supports
the use of this size)
- glue dot (prefer double dot as long as you can prevent moisture traps
for flux residue and other nasties) size and shape requires attention
- during touch-up/rework and repair operations do not allow the iron to
contact the end terminations
- handling procedures should also dictate caution
- lead finish was solder coating or fused SnPb.
Hope this helps.
Steve Sauer
Sr. Mfg. Engineer
Xetron Corporation
----------
From: Gabriela Bogdan[SMTP:[log in to unmask]]
Sent: Tuesday, October 06, 1998 1:44 PM
To: [log in to unmask]
Subject: [TN] Help on design rules for chip capacitors
Hello, TechNetters!
I am looking for information concerning design rules for ceramic chip
capacitors on the
wave soldering side of printed circuits.
I am interested in rules concerning the size, the termination finish and
general manufacturing technology.
If you can help me by giving any information, web sites or recommend
articles , I'll be
very grateful.
Thank you,
Gaby
ok
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|