Gary
I have had 2 or 3 clients having problems with LCDs a few months after
cleaning, although no one has ever given me an explanation. Just
practical experience. In the light of your experience, perhaps I should
modify it from "you cannot..." to "be careful and run life tests..."
Brian
Gary Camac wrote:
>
> Brian,
>
> Why do you feel you can't run LCDs through the wash? We have ran LCD displays through the
> wave and a soaponified wash for over 15 years here. I don't know of any field reliability
> issues on these units.
>
> I agree with Kelly's last comment on the inhale due to cooling the part too rapidly. This is
> the reason I like to see a slight temperature increase in each wet section of my washer.
>
> Gary Camac
>
> Phil Nutting wrote:
>
> > Hi all,
> >
> > I don't remember if I posted this question in the past months, but I'll
> > repost to get a fresh answer.
> >
> > Are there any components (pth) that can't be washed in an aqueous system?
> > Over the years we've had problems with electrolytics, polystyrene bodied
> > caps and small board mount relays.
> >
> > Does anyone have experience with thermal compound or other thermal
> > management materials in aqueous clean?
> >
> > Oh ya, the system I just installed is a closed loop DI water wash with no
> > chemicals.
> >
> > Phil Nutting
> > Manufacturing Engineer
> > Kaiser Systems, Inc.
> > High Voltage Power Supplies That Work(tm)
> > 126 Sohier Road
> > Beverly, MA 01915
> > ph: 978-922-9300
> > fx: 978-922-8374
> > [log in to unmask]
> >
> > ---------------------------------------------------------------------------------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> > Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> > ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|