TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 27 Jul 2005 09:46:03 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"Douglas O. Pauls" <[log in to unmask]>
In-Reply-To:
MIME-Version:
1.0
Parts/Attachments:
text/plain (75 lines)
Phil,
That question should probably go back to the make of the low residue flux.
I know that my friends at Kester and Alpha get asked to test compatibility
of fluxes to the wierdest things.  I have not every analyzed this
combination.  You should actually be asking two questions:  (1) what is the
effect of the oil on the flux residue, and (2) how tolerant is the
dielectric oil to trace amounts of flux residue without compromising
functionality.  The second question would have to go back to the maker of
the dielectric oil (or earl to our southern friends).

Doug Pauls
Rockwell Collins




             Phil Nutting
             <PNutting@KAISERS
             YSTEMS.COM>                                                To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             07/27/2005 08:46          [TN] no-clean flux "residue"
             AM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
               Phil Nutting
             <PNutting@KAISERS
                YSTEMS.COM>






Good morning,

Does anybody have experience with using no-clean cored wire solder on
through hole boards that will be submbeged in dielectric oil?

Thanks in advance,

Phil

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2