TECHNET Archives

May 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Craig Sullivan <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Craig Sullivan <[log in to unmask]>
Date:
Mon, 16 May 2011 10:45:57 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Hi Steve,

The ATS-667 is the St. Gobain M797 so this will also be supplied with a liner from now on. I just confirmed with Gary at ATS.
As mentioned, the lead times have also grown because of a scale-back on production. They are only making it when they have orders.

Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480
F: 607.266.0482
[log in to unmask]
 Please consider the environment before printing this e-mail.

-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Monday, May 16, 2011 9:52 AM
To: 'TechNet E-Mail Forum'; Craig Sullivan
Subject: RE: [TN] Conformal Coat tape

Hi Craig,

Try this:

http://www.ats24.com/store.asp?pid=31192

Polyester film with rubber pressure sensitive adhesive.

All-Spec carries it so you don't have to get a buy a whole log. I'm sure you can get some sampled to you to check out.

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Sullivan
Sent: Monday, May 16, 2011 9:34 AM
To: [log in to unmask]
Subject: [TN] Conformal Coat tape

Well, I suppose this is a repeat from a few years ago when Humiseal stopped selling their conformal coat tape and left everyone searching for alternatives.

Recap: Humiseal HT-500 tape was manufactured exclusively for Humiseal by St.
Gobain. The St. Gobain part number is M797. St. Gobain had numerous quality issues and as such Humiseal ceased the line. St. Gobain continues to manufacture the tape. We had continued to use the St. Gobain part with minor quality problems here and there. We decided to live with the issues because the tape works so well with our Acrylic coating.

Fast forward to today: St. Gobain decided to put the tape on a liner to correct various issues they and other customers had. Problem is we now see excessive residue left on the boards as well as the rolls falling apart if we're not careful with handling. They've also scaled back production and as such the lead times have quadrupled.

So, my question is can anyone share what they use with their acrylic coatings? We use a boat load of this stuff so I need to find a seamless replacement.

Thank you,
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480
F: 607.266.0482
[log in to unmask]<mailto:[log in to unmask]>
P Please consider the environment before printing this e-mail.


________________________________
Confidentiality Notice:
This e-mail contains privileged and confidential information which is the property of MPL Incorporated, intended only for the use of the intended recipient(s). Unauthorized use or disclosure of this information is prohibited. If you are not an intended recipient, please immediately notify MPL Incorporated and destroy any copies of this email. Receipt of this e-mail shall not be deemed a waiver by MPL Incorporated of any privilege or the confidential nature of the information.

Export Control:
This message is intended only for the addressee and may contain information that is company confidential or privileged. Any technical data in this message may be exported only in accordance with the U.S. International Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export Administration Regulations (15 CFR Parts 730-774). Unauthorized use is strictly prohibited and may be unlawful. If you are not the intended recipient, or the person responsible for delivering to the intended recipient, you should not read, copy, disclose or otherwise use this message. If you have received this email in error, please delete it, and advise the sender immediately.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 16.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2