Yep, as would say your gran-granfather.
Inge
----- Original Message -----
From: "John Maxwell" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, March 19, 2007 5:06 PM
Subject: Re: [TN] "Greenish colour on traces"
> Ingemar,
> We must also remember that nickel is magnetic as well increasing its
> impedance at high frequencies. That is a reason that many GHz passive
> components do not use a nickel barrier on their terminations.
>
> John maxwell
>
>
>>That's something else! You did not tell what purpose. It's right, for
>>some multiGHZ bands, where low losses are wanted, we don't use nickel
>>plating because it's higher resistivity. Some nickel platings can have
>>10 times higher losses than Copper and Gold! In these cases, we use just
>>copper (no plating at all)if it's possible in environmental point of
>>view, or we use tinned copper lines. So, silver over copper is
>>theoretically right. And metallurgically spoken, silver on copper has
>>been used for centuries. What I don't understand is why add gold. Maybe
>>to avoid silver tarnish, if the package is not hermetic.
>>Resistivity microOhm x cm :
>>
>>Electronic solder 17-20
>>Pure Tin 9-11
>>Electroless nickel 50-100
>>Electrolytic nickel 8-10
>>Electrolytic Gold 2.5
>>Copper lines 1.8
>>Electrolytic Silver 1.6
>>
>>When you look at the above table, you will understand why Silver.
>>
>>Inge
>>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|