TECHNET Archives

August 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="us-ascii"
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 17 Aug 2017 19:38:04 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Giamis, Andy" <[log in to unmask]>
Subject:
From:
"Giamis, Andy" <[log in to unmask]>
Message-ID:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (15 lines)
Hi Folks,
Has anyone had experience soldering to 'Nickel-Silver' 
This is a ternary alloy with approximately 60% Cu, 20% Ni, 20% Zn.

If so, are there any special considerations such as flux type, pre-tinning etc...



Best Regards,
Andy
Senior Failure Analysis Engineer