TECHNET Archives

August 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Kerry McMullen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 1 Aug 2006 09:56:33 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (113 lines)
Hi Franklin,
Thanks for the quick response.
After assembly.   We have also seen a bare board with thin hole wall Cu.

Thanks,
Kerry

Kerry McMullen
Principal New Product Mfg. Engineer
LTX Corporation
50 Rosemont Road
Westwood, MA 02090-2306
(T) 781-467-5468



Franklin D Asbell <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
08/01/2006 09:52 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Franklin D Asbell <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Barrel to Laminate Adhesion loss






Could be a few causes, at what stage are you seeing this?

1 - As Received condition?
2 - After Thermal Stress?
3 - After Assembly?

Some common causes could be;

1 - Poor drilling (resulting in excessive resin smear or damaged hole
wall)
2 - Poor resin smear removal
3 - Poor pre-electroless copper cleaning-prep
4 - Poor electroless copper plating
5 - Material type (are you using some exotic material)

Would you provide more info.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kerry McMullen
Sent: Tuesday, August 01, 2006 8:46 AM
To: [log in to unmask]
Subject: [TN] Barrel to Laminate Adhesion loss

Esteemed Tech-net,
What are the causes of Barrel to Laminate Adhesion loss?

TIA,
Kerry

Kerry McMullen
Principal New Product Mfg. Engineer
LTX Corporation
50 Rosemont Road
Westwood, MA 02090-2306

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
(T) 781-467-5468

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2