When I was involved with them I was unaware of any instances of Ag epoxies
supporting Ag migration. More recently work by Enthone on the similar
situation with their silver OSP finishes ['similar' meaning discrete
particles in an organic matrix] did not find this as an issue. Plasma
treated/activated is not referenced or in my experience and so is the
concern, anecdotally you can make the case below.
Possibly some thick/thin film guys or types from IMAPS might be more up on
this; plasma cleaning is often used by people in that zone. They might have
some references on this or maybe just some house rules built on experience.
Regards
Mike
-----Original Message-----
From: Hernefjord Ingemar [mailto:[log in to unmask]]
Sent: Tuesday, September 04, 2007 7:30 AM
To: [log in to unmask]; [log in to unmask]
Subject: RE: [TN] Plasma "oxidation"
Thanks, Mike,
another intelligent add to the discussion. The guys who 'invented' the
method of 'plasma oxidize' are both PhDs, one in Solid State Technology, the
other in Laser Physics. They performed tests with some substrates in that
they exposed these to damp environment plus voltage after the oxidizing. As
there was no silver migration, they had proven the idea.
With all respect, I'm not at all convinced. Migration and dendrite
formations are often hard to create in the lab. The reality life in the
field is different, as we all know. Testing a couple of samples is not
comparable with thousands of substrates in all kinds of situations.
Furthermore, oxidizing a few nanometers of silver on the silver epoxy dot's
surface does not inhibit possible migration paths from the underlying
millions of silver flakes. I think the whole idea is preposterous, or I'm
not learned enough to get it.
Thanks all for the contributions
/Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: den 3 september 2007 17:32
To: [log in to unmask]
Subject: Re: [TN] Plasma "oxidation"
I'm confused by this, probably because I'm not knowledgeable on plasma
cleaning. But so far as I understand this area, the principal uses of plasma
are
- ash off surface contamination to get a clean surface, Or
- it can be used to impregnate or burn surfaces to make them 'active'
(eg to make PTFE bondable with adhesive) It depends (!) on the type of
plasma and energies used.
This seems to be a confusion of these two functions. Oxidising epoxy would
make a carbon rich layer, oxidizing silver would make silver oxide, both AgO
and C are conductive so we have weakly conductive substrate.
This is a powered device so we have some volts,. The only missing item for
Ag migration is a little damp.
Altogether: not a recipe for high reliability. Or did I miss something?
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Friday, August 31, 2007 9:53 AM
To: [log in to unmask]
Subject: [TN] Plasma "oxidation"
Yup. Strange title. I've been asked about a strange process, which one was
introduced without my knowledge, and I'm going to throw it out. But I
thought of consulting TN before. This is the case:
LTCC substrates are silver epoxy dispensed for chip mounting. In order to
avoid risk for silver migration, a guy invented plasma "oxidation", i.e. he
use a plasma cleaner, runs Argon with 6% Oxygen for a couple of minutes on
mounted substrates. The silver epoxy dots become blackish because of
oxidation, and oxidized epoxy is meant to minimize risk for silver
migration. The oxide is of course just nanometer thick. The guy worked at a
wafer manufacturing plant and had experience of cleaning procedures.
I mean that this process is nonsense. If humidity gets in and condense on
the substrate, and if the electric field is high enough, and if there are
salts or contaminations, there is still enough silver to start migration.
Oxidation of the silver dot's surface is meaningless. Anyone heard of such a
strange process? Plasma operation on mounted LTCC substrates is foreign to
me, I want it out.
TrikeMan?
Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient please delete and
contact the sender by return and delete the material from any computer. Any
review, retransmission, dissemination or other use of, or taking of any
action in reliance upon, this information by persons or entities other than
the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness. In particular, Indium
Corporation does not accept responsibility for changes made to this email
after it was sent. Any opinions or recommendations expressed herein are
solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|