Are these components close to the edge of the board that has a scored rail?
In the event that it is I know of several customers that were having joint
failure when their components were too close to the board edge. Breaking off
the rail was enough to make a fracture. Their solution was to add in a
routed relief along the board edge where the score came too close. One board
was a heavy copper .093" thick multilayers with a .018" web thru FR4. I like
to see a thinner score web .012"-.015" for FR4 but the rails would come off
during their assembly process due to the weight build up. Other customers
were see it happen on .062" thick boards with the .012" web. Adding in the
routed stress relief seems to help them as well.
Regards,
David Duross
Quality Control Manager
Electropac Co.
252 Willow Street
Manchester, NH 03103-6294 USA
TEL (603) 622-3711
FAX (603) 622-1773
[log in to unmask]
----- Original Message -----
From: "Todd, Richard" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, January 11, 2007 6:03 PM
Subject: [TN] SMD Capacitor Shear Strength
>I have a question for the oracle . . .
>
> Does anyone know what is the solder joint shear strength for an 0603
> capacitor (assuming standard eutectic solder)?
>
>
>
> Regards,
>
>
>
> Rick Todd
>
> Senior Engineer
>
> Process Quality Engineering
>
>
>
> Panasonic Automotive Systems Company of America
>
> Division of Panasonic Corporation of North America
>
> 776 Highway 74 South, Peachtree City, GA 30269
>
> 770-515-1087 Direct
>
> 678-458-2887 Cell
>
> 770-486-2248 Fax
>
> [log in to unmask] <mailto:[log in to unmask]>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|