Richard is correct.
I would be very concerned about nickel leads. Years ago someone convinced
several captive PCB shops to use a nickel finish for SMT boards. We quickly
learned that nickel oxidizes in a heart beat and is difficult to remove.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Stadem, Richard D." <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, March 28, 2006 9:26 AM
Subject: Re: [TN] Nickel Lead Finish
Yes. Absolutely you should be concerned.
First, nickel alone cannot be used. There needs to be a protective alloy
over the nickel to prevent nickel oxides from forming. Standard
electronic fluxes do not work for nickel oxides.
Secondly, nickel is a poor surface to solder to. It has a much slower
dissolution rate than tin or tin-lead. It requires more heat over a
longer time in order to form a good intermetallic formation.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bloomquist, Ken
Sent: Tuesday, March 28, 2006 8:11 AM
To: [log in to unmask]
Subject: [TN] Nickel Lead Finish
We were just notified by one of our capacitor manufacturers that they
were going lead free and their replacement finish will be nickel. These
are surface mount parts.
If my memory serves we had trouble soldering nickel leads some years ago
on some TO-5 parts.
We are a class 3 manufacturer and will continue to use lead in our
solder. Should we be concerned about the solderability of the nickel
lead finishes?
Thanks,
KennyB
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|