Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wCpX7-000Bj2C; Thu, 3 Apr 97 10:38 CST |
Old-Return-Path: |
|
Date: |
Thu, 03 Apr 97 08:47:42 PST |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"8bYH73.0.UHK.AqzGp"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Thu Apr 3 11: |
07:01 1997 |
X-Loop: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Tamir,
You may need to look at how the gold is applied. If the gold is
applied in a deep gold process whereby the gold is an etch resist.
You may have copper suspended in the alkaline solution in the etcher
being redeposited on the surface of the gold. One way to verify this
is to have the surface analyized using Auger Electron Spectroscopy and
look for the presence of copper oxide on the surface. You can then
have an ion etch of 50 angstroms increments and verify if the copper
oxide (if there is any) is originating from below the surface or is
being deposited on the surface.
Regards,
Alan B. Cochrane
Director of New Technology
Multek Inc.
______________________________ Reply Separator _________________________________
Subject: Gold fingers-edge connectors
Author: [log in to unmask] at INTERNET_GATEWAY
Date: 4/3/97 5:57 AM
Hi
Lately we have some conductivity problems with the edge connectors.
It can be seen that after few hours at the open air the brightness of
the gold changed.There were few times that we got PC's from the
'field' with problems and after cleaning the edge connectors with an
eraser the problem was gone. First I want to know if any one deal
with the same problem and if anyone can tell me if there is any
differences between the definitions of the gold/nickel thickness of
the IPC600 & IPC610 standards.
Thanks
Tamir
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|