I now have a customer asking us not to use Immersion Silver due to
migration. Isn't this old news? I thought the benzomidazole and other
organic inhibitors prevented Silver migration.
Dave C.
-----Original Message-----
From: David D. Hillman [mailto:[log in to unmask]]
Sent: Wednesday, June 16, 2004 5:49 PM
To: [log in to unmask]
Subject: Re: [TN] Yellow Discoloration of Immersion Silver Boards
Hi Rich! I recommend getting a copy of Lenora Tuscano/Don Cullen's paper
given at the IPC 2003 Fall meeting titled "The Study, Measurement, and
Prevention of Tarnish on Immersion Silver Board Finishes". The paper
documents that the "yellow" tarnish found on immersion silver pwbs used in
the study, using SERA and ESCA analytical techniques, can be silver
sulfide, is in the thickness range of 200-500 angstroms, and is still quite
solderable (lots of info in the paper - this is the reader's digest
version). As others in our TechNet community have discussed, the yellowing
can be a typical visual appearance. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Richard
Kraszewski To: [log in to unmask]
<[log in to unmask] cc:
COM> Subject: [TN] Yellow
Discoloration of Immersion Silver Boards
Sent by: TechNet
<[log in to unmask]>
06/16/2004 09:13
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
Richard
Kraszewski
We are seeing yellow discoloration of Immersion Silver Boards right out
of the package from our board house. They seem to solder fine, however
this is causing some concern with our customer. I suspect that it could
be a thin film of silver bromide or silver carbonate both which are
yellow powders.
Any one seen this before?
What is it?
How does the board house remedy this situation?
Any associated concerns or other bits of wisdom?
I would truly appreciate any input.
Rich Kraszewski
Advanced Manufacturing Engineer - KEDS
Phone: 260.925.8919
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|