Why would open (assuming you mean unplugged) immersion silver vias
increase assembly problems and cost more money?
Should immersion silver vias be plugged as a standard all the time?
Kaye Clayo
Keithley Instruments, Inc.
At 11:39 AM 6/11/2005, you wrote:
>We have been manufacturing boards with immersion silver for 8 years, six
>of those we have supplied plugged vias.
>The process works best BEFORE the immersion silver process. It should not
>be done after immersion silver because of the possibility of contaminating
>the silver.
>There NEVER should be anything in the via holes that could etch the hole
>walls. They must have a very marginal via plugging process. Best pick
>another fabricator until they improve their via plugging. Open vias could
>increase assembly problems and cost you more money.
>
>Happy Holden
>Westwood Associates
>
>
>
>
>Kanaiyalal Patel <[log in to unmask]>
>Sent by: TechNet <[log in to unmask]>
>06/10/2005 05:23 PM
>Please respond to
>TechNet E-Mail Forum <[log in to unmask]>; Please respond to
>Kanaiyalal Patel <[log in to unmask]>
>
>
>To
>[log in to unmask]
>cc
>
>Subject
>[TN] Immersion Silver - Via Plugging
>
>
>
>
>
>
>Our supplier is recommending against plugging via holes the immersion
>silver boards and here is their explanation. Need some input into how you
>guys are managing.
>
>"We can not plug before silver because chemicals used during the silver
>process may become trapped. Over time these chemicals can eat away at the
>hole wall copper creating voids.
>2. Because the boards have passed through rout and are in piece form when
>silver is applied the board can not be plugged in panel form as are the
>gold boards.
>3. Immersion silver is soft and easily damaged. It is our last
>manufacturing process and we avoid handling it as much as possible after
>being coated, this particularly applies for the plug process."
>
>Appreciate your feedback.
>re,
>Hemant
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>_____________________________________________________________________________
>Scanned by IBM Email Security Management Services powered by MessageLabs. For more information please visit http://www.ers.ibm.com
>_____________________________________________________________________________
CONFIDENTIALITY NOTE: This message is intended only for the use of the individual or entity to which it is addressed and may contain information that is privileged, confidential, and exempt from disclosure under applicable law. If the reader of this notice is not the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify the sender immediately.
_____________________________________________________________________________
Scanned by IBM Email Security Management Services powered by MessageLabs. For more information please visit http://www.ers.ibm.com
_____________________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|