TECHNET Archives

September 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 12 Sep 2012 06:37:44 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Douglas Pauls <[log in to unmask]>
X-cc:
In-Reply-To:
<632462C8BC644D6B832E6619DED527B2@MikeLaptop>
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (86 lines)
Speaking of formates, perhaps Rich has ants running around on his 
assemblies.  We had an assembly come into a service center from Brazil 
crawling with ants which we found exude high amounts of formic acid.

Doug Pauls



From:   Mike Fenner <[log in to unmask]>
To:     <[log in to unmask]>
Date:   09/11/2012 02:34 PM
Subject:        Re: [TN] Source of IC Contamination Species
Sent by:        TechNet <[log in to unmask]>



I think you have the answer from other posters, so for information to
complete the picture:
Some fluxless die attach in high power devices is done using formic acid.
The acid is injected into the (inert) furnace atmosphere at the beginning 
of
the reflow cycle. Formic is used because it breaks down completely at 
(from
memory) around 110C to H20 and CO2. 
This being the case formates are unlikely to be present after reflow, 
making
the probability high that they are being introduced later or generated
elsewhere as postulated.


Regards


Mike Fenner

Bonding Services & Products
M: +44 [0] 7810 526 317
T: +44 [0] 1865 522 663
E: [log in to unmask]

 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Tuesday, September 11, 2012 5:10 PM
To: [log in to unmask]
Subject: [TN] Source of IC Contamination Species

Occasionally, IC analyses are reported to have elevated levels of acetates
and formates.   Is it the general consensus that source of these
contamination is assumed to be the decomposition of larger molecular 
weight
weak organic acids found in soldering fluxes?  I can't imagine that any
manufacturer would actually be placing acetic or formic acids directly 
into
a flux formulation. These are much too volatile and aggressive. 

Thoughts?

Rich  Kraszewski 
Senior Process Engineer
PLEXUS 
 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2