TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vPcAn-0000WGC; Mon, 18 Nov 96 16:28 CST
Content-Type:
text/plain; charset=US-ASCII; X-MAPIextension=".TXT"
Old-Return-Path:
Date:
Sat, 21 Sep 96 07:18:43 GMT
Precedence:
list
Resent-From:
Message-ID:
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/7804
TO:
Return-Path:
<TechNet-request>
X-Status:
Resent-Message-ID:
<"5OHUG2.0.iBD.yBEao"@ipc>
Subject:
From:
Nathan Barnes <[log in to unmask]>
X-Loop:
From [log in to unmask] Tue Nov 19 09:
35:32 1996
Content-Transfer-Encoding:
quoted-printable
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (45 lines)


Here are some illustrative  numbers  which show that you shouldn't have to do
too much to get a result. These numbers are illustrative only. The dispense
parameters you actually require will depend on your adhesive type and equipment.


Component		0603	0805	1206	
Needle ID (mm)		0.33 	0.4	0.4	
Dispense height (mm)	0.1	0.1	0.1	
Dot diameter (mm)		0.55	0.8	0.9	
Diameter Tol (? mm)	0.75	0.1	0.1	
Dispense Pressure (Bar)	3	3	3	
Delay Time (ms)		50	50	80	

Mike Fenner
BSP

-----------------------------------------------
Pat McGuine wrote:
> 
> Hello:
> 
> We have a new design that has 0805s on the bottom of a board that will be
> wave soldered.  We have done 1206s for years but our dot for the 1206s is
> too large for the 0805s......

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2