A technique I've seen used to get into the inner layers of a ML board
uses a dentist's drill. The bit spins at around 400,000RPM on compressed
air bearings and the tungsten tip gives absolute and total control. I
saw a technician excavate his way into the centre layers of an 8 layer
board using an ordinary illuminated bench magnifier for precision, and
the result almost blew me away. I had a go at it myself, and the degree
of control is astounding. I guess just as well - you would want your
dentist to have absolute control, right?
By the time he'd finished his repair, I was hard pressed to find the
point of entry as the cut had minimal width and no extraneous damage.
--
Cheers
.......Andy K.
=======================================================================
Andy Kowalewski Phone: +61 3 9264 3767
PCB Design Engineer Fax: +61 3 9264 3507
NEC Australia email [log in to unmask]
Mobile: Australia 0412 281 284
International +61 412 281 284
=======================================================================
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|