Hello Clive,
I've never personally used an S-glass board but I have come across
a some info on it in years past.
It is described as a fibreglass reinforcement that is attractive in
aerospace applications because it is lightweight yet a superior weave.
It is said to have a good balance between tensile, flexural and
compressive strengths.
You may find more at fibreglast.com or perhaps another material vendor's
web site.
John Denton
Omni PWB
Clive Ffitch wrote:
>
> Hi All,
>
> Does anyone out there have any information or specification details on
> "S-glass" fibre reinforcement material as used in PCB laminates, and
> what does the "S" stand for?
>
> There are TCE (sorry CTE for you guys!) advantages with its use, and
> depending on the resin system it is used with, Er advantages also, but
> I am looking specifically to identify and understand the differences
> between "S-glass" fibre material and the more conventional "E-glass"
> fibre material. (I understand "E" stands for "Electronics" Grade???).
>
> How many people use S-glass?
>
> What benefits do you see?
>
> Any comments appreciated.
>
> Clive ffitch
> Matra BAe Dynamics UK
> Stevenage, England
> E-mail [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|