TECHNET Archives

February 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Graham Naisbitt <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 25 Feb 2002 10:37:01 -0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (131 lines)
Yes, me too! Please fix it Steve?

Regards Graham Naisbitt

[log in to unmask] <mailto:[log in to unmask]>

Concoat Limited
Alasan House, Albany Park
Camberley GU16 7PH - UK

www.concoat.co.uk <http://www.concoat.co.uk>

Phone: +44 1276 691100
Fax: +44 1276 691227
Mobile: +44 79 6858 2121


> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of
> [log in to unmask]
> Sent: 25 February 2002 01:05
> To: [log in to unmask]
> Subject: Re: [TN] Dendritic Growth...
>
>
> Hi, Steve,
>
> Just tried looking up your site to see these beautiful dendrite pictures,
> but found you have a bully muscling in on your link. Instead of getting to
> your site I was beamed off to http://www.megago.com/l/, who then asked me
> if I wanted to make them my home page. S.. Off! I thought, but I had to
> type your site address manually to get to the pictures.
>
> Anyone else had this problem?
>
> Peter
>
>
>
>
>
>                     SteveZeva@AOL
>                     .COM                 To:     [log in to unmask]
>                     Sent by:             cc:     (bcc: DUNCAN
> Peter/Asst Prin Engr/ST
>                     TechNet              Aero/ST Group)
>                     <[log in to unmask]        Subject:     Re: [TN]
> Dendritic Growth...
>                     ORG>
>
>
>                     02/23/02
>                     02:49 AM
>                     Please
>                     respond to
>                     "TechNet
>                     E-Mail
>                     Forum.";
>                     Please
>                     respond to
>                     SteveZeva
>
>
>
>
>
>
> Hi Phil!
>
> The pictures are up! Go to:
>
> http://www.stevezeva.homstead.com
>
> Those are the best examples of dendritic growth as I've ever seen! Where
> did this take place? In a SIR chamber?
>
> -Steve Gregory-
>
>
>  Hi Steve,
>
>  Thanks for offering to post my pictures of the dendritic growth.  It will
>  be interesting to see what the consensus is although since I sent the
>  email
>  out I have been able to get my hands on the defect and take a
> close enough
>
>  look to answer the question.  Let's put the picture up and see what the
>  responses are.
>
>  Phil
>
>
>
>
>
> [This e-mail is confidential and may also be privileged. If you
> are not the
> intended recipient, please delete it and notify us immediately; you should
> not copy or use it for any purpose, nor disclose its contents to any other
> person. Thank you.]
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2