In a message dated 5/13/00 1:15:05 AM US Eastern Standard Time,
[log in to unmask] writes:
<< From your description, it seems likely your halides are inorganic. As
such, they are readily ionised and a cheap way of doing the tracing is
with an ionic contamination tester (e.g. Contaminometer, Omega Meter,
etc...). >>
Unfortunately, the bulk ionic testers you reference fall short of telling you
how much of what halide exists. Thererfore, bulk ionic testers tend to be
limited to monitoring process control. A systematic analysis requires a much
more precise method. One such method is ion chromatography. This method can
easily determine how much of a halide is present in solution, such as
chloride. bromide, sulfate, and weak organic acid (activators in fluxes,
particularly low solids, no-clean fluxes) at a given point in the
manufacturing process.
Hope this helps.
Dave Morrow
Contamination Studies Laboratories, Inc.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|