Ed,
Unfortunately access was denied but on a general note metal particles on
MLCC surfaces are some what common and are due to several factors. First,
typically these parts are vibratory bowl fed to a tape a reel machine for
reeling and depending on vibration intensity and chip size, parts
terminations will mark the bodies of other parts. Second, surface roughness
plays a significant factor in termination marking. From a practical stand
point this marking becomes less desirable as operating voltages increase,
spacing shrinks and if moisture, contamination etc. is present to promote
nasties to form between metal marks between MLCC and PWB.
John
At 08:21 AM 6/3/02 -0700, you wrote:
>Fellow Technetters,
>
>I recently found extraneous metal on the surface of several MLCCs on an
>assembly. I examined stock parts and found this condition pre-existed on
>the stock caps (tape & reel). These caps have pure tin terminations. There
>is a picture of this condition at the link below ...
>
>http://www.eskimo.com/~ehare/MetOnCap.bmp
>
>What is your opinion of the acceptability of this condition?
>
>What might be the root cause?
>
>Are there any specifications that address this issue?
>
>Best regards,
>Ed
>--
>
> SEM Lab, Inc.
> Scanning Electron Microscopy
> and Failure Analysis
> Snohomish, WA
> Ph. (425)335-4400
> Fax (603)658-4519
> http://www.semlab.com
>
>---------------------------------------------------------------------------
>------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
>SET Technet NOMAIL
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>---------------------------------------------------------------------------
>------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|