TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], Hernefjord Ingemar <[log in to unmask]>
Date:
Wed, 28 Nov 2007 10:28:48 -0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (98 lines)
 
Ing: With respect to dust is it primarily a question of
breakdown/penetration of the polymer?  I can't now find the reference but I
am sure that I have read a study by  Per-Erik Tegehall of your IVF  which
showed that with dust a cause of coating failure was a conductive dust layer
ON the coating. Shouldn't be too hard for you to dig out as they are just up
the road (in global terms) from you.


Regards 

Mike 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Tuesday, November 27, 2007 10:03 AM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coating Breakdown and Iraqi dust

David,

Thanks for reports. I also have your book. 

Now, in one of the reports (page 17)there is a test on Polyethylene and
Intercept(TM). It says, that it takes 7 days for a 1 ppm Chloride
environment to breakdown Polyethylene, while it takes 35 years for the
Intercept. In both cases the film thickness is 2 mils. This has two sides,
one surprising and one frightening:

1. Is Intercept really that superior?

2. If Polyethylene is out after only 7 days, then what about acrylic
coatings, e.g. Humiseal 1B31? Will Chloride ions penetrate after only a
number of days, rather than years?

Furthermore, on page 17, 1 ppm Chloride is named 'normal environment'.
Who said that?

The dust from Iraq has up to 0.4 weight% of Sulphur or Chlorine (EDS).
If 1 ppm of Chloride penetrates 2 mils of Polyethylene in 7 days, then 0.4%
of Chlorine(Chloride)sounds to me like catastrophic!

What's the expert's opinion? I suppose there is no such experts in this
forum, but you may at least have an idea.

/Inge

-----Original Message-----
From: David Douthit [mailto:[log in to unmask]]
Sent: den 26 november 2007 19:05
To: TechNet E-Mail Forum; Hernefjord Ingemar
Subject: Re: [TN] Conformal Coating Breakdown and Iraqi dust

Inge,

Attached are 2 reports that should give you a better idea of the hazards you
are facing.

The first is titled "Avionics Systems, Reliability, and Harsh Environments"
June of 2001

The second is titled "Static Intercept and Corrosion Intercept" by Lucent
Technologies.

You have serious issues!

David A. Douthit
Manager
LoCan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***"

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2