Dean
Heck, you can solder untarnished steel with 63/37.
Substantial issues relating to fluxing and defluxing aside, low-alloy steels
have ~2% weight of refractory materials [ie, Si, Cr, Mn, etc] that are very
difficult to solder.
Dave Fish
----- Original Message -----
From: "May William D (Dean) CNIN" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, April 08, 2002 6:47 AM
Subject: [TN] Solder alloy for 1010 Steel
> We have some 1010 cold rolled steel board stiffeners that require
soldering
> to a circuit card like a through-hole part. Does anyone know if there are
> any solder alloys that will wet to 1010 steel? We could have them
> electroplated with tin/lead to make them solderable but was curious if
there
> was an alternative.
>
> Thanks for your consideration!
>
> Wm. Dean May
> NSWC Crane
> Bldg. 38, Code 6086
> 300 Highway 361
> Crane, IN 47522
> 812-854-3073
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|