TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Roger Massey-G14195 <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 10 Mar 1999 09:20:21 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (41 lines)
     Hi TN,

     Has anybody out there in the "real world" ever had cause to solder a
     BGA onto a socket so that it turns into a Pin Grid Array?  I need to
     make up some test boards for a customer, and we dont have the BGA at
     the minute, but the electrical folks want to test their design without
     waiting for the BGA to arrive.  Some body found a supplier who can
     supply an adaptor, which is essentially a piece of FR4 with enough
     pins to cover all the balls.  One end of each pin has a small cup to
     take the ball, while the other is a standard pin.

        It seems a simple enough idea, place the BGA and reflow,  has
     anybody done this before, or something similar?
        Do you think it likely that the I will need more solder paste in
     the cups?  Looking at the cup size, and the ball size I think I may
     have to add some paste, but the cups stick up nearly 2mm from the FR4,
     so printing is not really that suitable,  could dispensing be a better
     bet (dont have any experience in that!)

                Any help would be appreciated,

                        Thanks
                           Roger


     Roger Massey
     Motorola AIEG
     UK

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2