TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vPVVk-0000XkC; Mon, 18 Nov 96 09:21 CST
Content-Type:
text/plain; charset=US-ASCII
Old-Return-Path:
Date:
Mon, 18 Nov 1996 09:23:37 -0600
Precedence:
list
Resent-From:
Message-ID:
Content-Transfer-Encoding:
7bit
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/7778
TO:
Return-Path:
<TechNet-request>
From [log in to unmask] Mon Nov 18 13:
31:11 1996
X-Status:
Content-Description:
cc:Mail note part
Subject:
From:
X-Loop:
Mime-Version:
1.0
Resent-Message-ID:
<"n-kPx3.0.hEK.px7ao"@ipc>
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (26 lines)
     Address,
     
     Other than book knowledge, I don't have a lot of hands-on experience 
     with SnPb Oxidation (other than finding it, SEC Test).  Since I am 
     having difficulties in finding a local source to Re-HAL some internal 
     PCBs, I thought I'd approach this matter from another direction.  
     
     Within a FAB Shop, copper oxidation can be easily removed with Sodium 
     Persulfate (Microetch) should this condition present itself.  
     
     What chemicals would you use to remove SnPb Oxidation?
     
     Please advise.  Thank you.
     
     John Gulley  - QA
     972-578-3928

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2