TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 9 Aug 2004 13:38:12 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Crepeau, Phil" <[log in to unmask]>
Parts/Attachments:
text/plain (49 lines)
hi,

i don't know the exact conditions of  your pwb, but might it not be possible to run it through a solder dip and hot air leveling operation?

phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Cheryl Tulkoff
Sent: Monday, August 09, 2004 12:45 PM
To: [log in to unmask]
Subject: [TN] Removing solder from PTH barrels


Does anyone have any clever suggestions on how to get solder (all of it)
out of .024" diameter PTH barrels?

The barrels are supposed to be completely clear of solder since they are
used for a press-fit connector.  There is just enough solder in the holes
to keep the connectors from seating properly. The barrels ended up with
solder paste in them after some boards were run using the wrong stencil.
The operator wiped the boards by hand towards the holes forcing some
solder paste into the barrels. He didn't follow up with a clean either.

While I'm at it, does anyone have a really good process for cleaning
misprinted boards? Obviously, our current procedure wasn't followed but
maybe someone has a better way.

Thanks, Cheryl

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2