We were given some boards from one of our customers, that we normally would
not do because of the fine pitch IC(20mil). Our printing process didn't do
bad considering the situation, but it did cause some soldering problems that
I'm trying to fix. This board is double sided with two 41 pins 20 mil
spacing IC's next to each other. The soldering problems that I am having is
insufficient solder on some of the pins due to poor printing. Since there
are parts on each side, does anyone have any recommendations on how to add
solder to the pins with insufficient solder? How does it get done on the
fine pitch side of manufacturing? What equipment is needed to add solder to
the pins?
Any advise would be greatly appreciated!
Jim
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|