Good old days, att lab got a paper outlined allowable rework that showed rework temp, time effect the reliability (set limit to allowable using accelerate life test to define it). IMC got higher resistance compare to the solderjoints. Thick IMC would eventually resulted high resistance joint, either by void formation or resistance change. You need to define it as your product requires. (For something that in the space, for example, you can not get customer repair and overhaul easily, caution should be taken. For a toy for your kid or 5 dollar watch, may not matter - provide you are not on road to airport.
--------------------------
Sent using BlackBerry
----- Original Message -----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Thursday, June 02, 2011 09:19 AM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Re-balling BGAs
I'm sorry, but I completely disagree with that logic. Rework is defined as bringing a component or CCA into full compliance with print requirements. If I have a BGA with SAC alloy balls, remove the SAC balls and re-attach Sn63 balls and use that re-balled BGA on a CCA whose print requires Sn63, then it is rework, not repair.
One does not need to follow the original manufacturing method. That is completely irrelevant.
You can rework a CCA (or a component) using hot gas, hot air, laser, solder iron, selective solder, selective vapor phase soldering, and any number of other methods.
By your definition, any touchup done with a solder iron on a board that had been vapor-phase soldered would be considered a repair, and thus would require approval by the customer. Do you do that?
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, June 02, 2011 6:08 AM
To: Stadem, Richard D.
Subject: RE: Re-balling BGAs
June 2, 2011
Because re-balling is not the original manufacturing method used by the
part manufacturer and the difference between repair and rework is when
you follow the original manufacturing method (like replacement of a part
soldered on an assembly) it is considered a rework and not a repair.
However, if you are not following the original manufacturing method it
is considered a repair and therefore the process of re-balling is a
repair not a rework.
-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Wednesday, June 01, 2011 5:43 PM
To: TechNet E-Mail Forum; Bogert, Gerald L (Contractor)
Subject: RE: Re-balling BGAs
Why would it be a repair?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerald Bogert
Sent: Wednesday, June 01, 2011 2:22 PM
To: [log in to unmask]
Subject: [TN] Re-balling BGAs
June 1, 2011
Anyone have technical data to support (or not support) re-balling of
BGAs to change from SAC balls to Pb balls???
My understanding is that because of the extra heat cycle involved, BGA
manufacturers may not stand behind their part warranty if re-balling is
done. I also seem to recall a technical poster or paper presented at
IPC several years ago which I believe indicated a reduction in
reliability of the part if it is re-balled.
Also seems to me that if one were to re-ball a BGA, this would be a
repair and not a reqork process and as such may require specific
customer approval.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|