All,
Great explanation. Thanks for clarifying this. It seems like most CMs
however, are focused on the TAL using 183 C as a starting point, which
the SnPb paste manufacturer's recommend.
Best Regards,
-joe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, January 07, 2008 9:14 AM
To: [log in to unmask]
Subject: Re: [TN] Reflow profile development - correct starting
temperature for evaluating TAL using non-eutectic solders
To build on Werner's comments, understand that you must be in total
liquidus for wetting dissolution (IMF formation) to take place. No real
wetting takes place in the plastic range between 179 and 189 C. The
difference is somewhat irrelevant, as you should really be above at
least 189 (liquidus) plus 20C as Werner stated. So your TALT should
begin at 209C ramping up and again ramping down. You really do not need
to have this TALT be longer than 15 seconds or so for good wetting on
the coolest solder joint on the assembly, even on ENIG. If this means
having a TALT longer than 120 seconds on the hottest point, then make
sure you use nitrogen else if the solder is held in liquidus for that
long of a time some oxidation begins to occur (just like the dross
formation on your wave solder or tin pot) and you get overheated,
flux-starved solder joints.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*
Sent: Monday, January 07, 2008 10:56 AM
To: [log in to unmask]
Subject: Re: [TN] Reflow profile development - correct starting
temperature for evaluating TAL using non-eutectic solders
Hi Joe,
Unfortunately, a natural outcome of a proper reflow profile has become a
parameter to be aimed at. TAL is NOT a proper reflow parameter, and
assures in and of itself not good wetting and metallurgical bonding.
Adequate solder joint quality is assured with achieving Liquidus+20 C
for 5 seconds at the slowest heating solder joint in the assembly. So
whatever the Liquidus temperature is for your solder alloy +20 for 5
seconds. For eutectic SnPb that means 203C for 5 seconds at the slowest
heating solder joint, which of course means everything else on the
assembly will see higher peak temperatures for longer times [except for
vapor phase, of course].
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
**************
Start the year off right. Easy ways to stay in shape.
http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|