My two cents worth. If I remember correctly there is a section in the
J-STD-001 Handbook that list the different types of metals used in making
leads and Alloy 42 shows it contains more iron than the other material (I
think it is Kovar) that has been used in the past. Someone told me it that
Alloy 42 was developed for reducing cost of materials. It reduce the amount
of nickel being used I believe, if my memory serves me correctly, Jon
-----Original Message-----
From: Ron Waugh [mailto:[log in to unmask]]
Sent: Thursday, November 02, 2000 7:28 AM
To: [log in to unmask]
Subject: [TN] Alloy 42
Technetters,
I have a huge problem with the wetting and solderability of a fine
pitch 15 mil QFP. I then spoke with the solder supplier; which
requested a couple of the components and performed x-sections. During
the x-sections, they also performed a metal composition of the
components lead. The metal in the leads turned out to be alloy 42,
which is ....non-wetting???? ...."or so I'm told".
I really don't know much about metals but the solder supplier stated
that the component will never wet properly. I would really like to
get some literature on this alloy 42 and ask if anyone else has had
any of these problems and what was their fix.
Thanks in advance for your time and energy.
Regards,
Ron Waugh
Process Engineer
Diversified Systems, Inc.
Phone: (317) 299-9547 Ext. #336
Fax: (317) 298-2055
Email: [log in to unmask]
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|