TECHNET Archives

February 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 27 Feb 2009 13:59:19 -0500
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gervascio, Thomas L" <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"Gervascio, Thomas L" <[log in to unmask]>
Content-transfer-encoding:
7BIT
Parts/Attachments:
text/plain (29 lines)
Have a problem and curious to see if others have the same problem.
Misery loves company you know. We have some MELFs that are moving during
reflow. They are not tombstoning and the direction of movement is
perpendicular to the direction of travel . The parts are properly placed
prior to reflow but are sliding off the pads along the edges of the
pads. It seems like something is happening during reflow that is
disturbing the MELFs. No indications of any other parts being skewed.
The MELF pads are the U-shaped pads to help reduce tombstoning. Don't
think I can change to a non eutectic tin/lead solder paste (a paste with
a plastic range) but if the parts are indeed being disturbed by
vibration I don't know if that would help. 



Tom 
 



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2