NASA Reference Publication 1124, Rev. 4 published by Goddard Space Flight
Center gives FR4 A TML rating less than 0.42 and a CVCM less than 0.01.
Outgassing limits are TML less than 1.0 and CVCM less than 0.10 for space
and high vacuum applications.
-----Original Message-----
From: Dan R. Johnson [mailto:[log in to unmask]]
Sent: Thursday, March 27, 2003 1:35 PM
To: [log in to unmask]
Subject: [TN] FR-4 outgassing
I looked through the archives and didn't see any information on out gassing
from FR4. I have a customer who has requested a part with no outgassing.
I can contact Rogers and GE for tech info on Rogers 4053 and Getek, but
really don't have a clue who to contact about generic FR4 out gassing
characteristics. Can anyone out there provide any insight?
Thanks,
Dan
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|