TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
John Guy <[log in to unmask]>
Reply To:
Date:
Mon, 10 Nov 1997 15:49:50 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (76 lines)
Legend,
        If you aren't using Nitrogen at this time and you haven't changes pastes,
there should be no reason to start using it now.
        Will the profile change.  The answer to this has two sides.  First, does
the paste manufacturer you are working with want you to use a different
profile for BGAs.  Some do.  You best bet is to contact your paste
manufacturer and ask.  Second, even if the reflow profile requirements
don't change, your oven settings probably will.  This is because most
reflow systems have a hard time getting heat to the balls under the
component.  This is not that big a deal, but it is something to keep in
mind.  Your best bet on this one is to instrument the solder joint that you
think will be the coldest on that component and run a profile through your
system and make any changes that may be needed.

Hope this helps,

John Guy
ACI / EMPF
714 N. Senate Ave.
Indianapolis, IN 46202-3112
voice:  (317) 655-EMPF ext.130
fax:    (317) 655-3699
e-mail:         [log in to unmask]


-----Original Message-----
From:   Legend Zhang [SMTP:[log in to unmask]]
Sent:   Friday, November 07, 1997 10:15 AM
To:     [log in to unmask]
Subject:        [TN] BGA soldering profile

Dear Technetters,

Is Nitrigen enviroment essential to BGA(144 pin) reflow
soldering? Should there be any difference between BGA and
general QFP reflow soldering profile? Any feederback would
be appreciated.

--

Best regards,

******************************************************
|          Legend Zhang (Li Zheng)
|          Morolola Cellular, GCCSD
|          Tel: 847-523-1017(O)
|          Fax: 847-523-8796
|          Pager: 847-576-0295, pin:18585
*******************************************************

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2