> I would suggest that 85/85 be used rather carefully.
>
> If you're testing low solids fluxes you may get a false "warm fuzzy."
>
> Many activators used in low solids no-clean evaporate at 85 C. From the SIR
> it looks like you're doing good. But in the real world, i.e. non-85
> operating conditions, your product may have problems. (See John Sohn's work
> published I believe at an IPC conference.)
>
> Also I would not recommend testing boards with plated through holes at
> 85/85. Lando et al (many years ago) showed that CAF is the dominant failure
> mechanism under these conditions especially if there is any bias.
>
> I am not a big fan of 85/85 although I had to do a lot of it over the years.
>
>
> I'd be interested in others opinions on the subject.
>
> Greg Munie
>
Techies,
May I just add my endorsement to Greg's comment. If you are testing no-clean
fluxes, it has been shown that 40DegC 93%RH is a more important condition.
Once flux residues are exposed to temperatures above around 40 to 50 C, they
volatise - hence the "warm fuzzy" Greg refers to. (BTW, this is not an
approved expression here in old Blighty!) :-)
--
Regards, Graham Naisbitt
[log in to unmask]
Mobile: +44 (0)79 6858 2121
Concoat Limited - Engineering Electronics Reliability
Web: www.concoat.co.uk AND www.concoatsystems.com
NOTE: NEW ADDRESS :NOTE
Sales:
Millfield House, Fleet Road
Fleet, Hampshire GU51 3QF UK
Phone: +44 (0)1252 813706
Fax: +44 (0)1252 813709
Manufacturing and Head Office:
Alasan House, Albany Park
Camberley, Surrey GU16 7PH UK
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|