Oh absolutely.  Another example of re-learning is that the University of Iowa found Vanadium at roughly 270PPM was a critical alloying element in Damascus steel.  Ironically this is very close the to percent of Vanadium in Swedish ores offering further proof that the Vikings regularly traded with the Middle East.