Jack, I'm not a materials guru, but I think the 4.7 is for the resin alone,
whereas the 4.2-4.3 is the combination of Eglass and resin and more accurately
represents the core material.
Jana Carraway
Maxtek Components Corporation
"Olson, Jack C" <[log in to unmask]> Wrote:
|
| WARNING: this is a very unexciting question...
|
| My software does some basic signal integrity analysis,
| and I just noticed it defaults the dielectric constant for
| regular FR4 to 4.7
|
| I was under the impression that most FR4 is at 4.2-4.3
| these days (more resin? thinner cores? can't remember...)
|
| Even a brief response will be appreciated!
|
| Jack
|
| ##########################################################
| ######
| TechNet E-Mail Forum provided as a free service by IPC
| using LISTSERV 1.8c
| ##########################################################
| ######
| To subscribe/unsubscribe, send a message to
| [log in to unmask] with following text in the body:
| To subscribe: SUBSCRIBE TechNet <your full name>
| To unsubscribe: SIGNOFF TechNet
| ##########################################################
| ######
| Please visit IPC web site (http://jefry.ipc.org/forum.htm)
| for additional information.
| For the technical support contact Dmitriy Sklyar at
| [log in to unmask] or 847-509-9700 ext.311
| ##########################################################
| ######
|
|
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|