Glenn,
The problem with using them with tin or tin-lead is that the quite stable
layer of oxide that forms on tin can result in poor conduction. If you
melt the tin/tin-lead during epoxy cure then the silver filler in the
epoxy may leach into the solder, leaving a silver depleted and therefore
non-conductive layer of adhesive - I have heard of people getting away
with this through very carefull process control, but I think it would be
better not to risk it if possible. I believe the adhesives engineered to
work with tin have "hard spiky bits" to penetrate the oxide layer.
David Whalley
>David,
>Very interesting. What would be the reasoning for not using silver-filled
>epoxy with tin or solder surfaces?
>
>Glenn Pelkey
>Quality/Reliability Engineer
>| The general rule for using silver filled epoxys is not to
>| use them with tin or
>| solder finishes. Some manufacturers do market materials
>| designed to work with
>| them and I have also talked to people who have had success
>| with other materials
>| by very carefully controlling the curing process so that
>| the solder layer just
>| briefly melts, but if you can switch to another finish on
>| the wire you are less
>| likely to have problems.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|