Hi Werner,
I like your thinking but...
I'm not in the quality department, no offense to those of you who are, but I
wouldn't want to be ;-) But thinking like an inspector, how would you verify
that you got the right size holes if you don't call out a finished hole
size? I guess you could do a cross section but a pin gage is a lot simpler.
Just thinking out loud,
KennyB
-----Original Message-----
From: Werner Engelmaier /* [mailto:[log in to unmask]]
Sent: Monday, July 07, 2008 3:36 PM
To: [log in to unmask]
Subject: Re: [TN] Flex specifications - tolerance on hole size
Hi Graham,
Why do you care what the finished hole size is? Do you put component leads
into 0.028"/+- 0.003" holes, that is 25 mils minimum?
The finished hole size specifications are an anachronism harking back to the
THT-days-today they only should be specified for componet lead holes. For
vias
the drilled hole diameter should be specified-it is much more important.
Werner
Future workshops:
Pb-Free Soldering Processes-Survival, Quality, Reliability, July 17/18,
Thal,
Switzerland
Pb-Free Soldering Processes-Survival, Quality, Reliability, July 21/22, Bad
Segeberg, Germany
Pb-Free Soldering Processes-Survival, Quality, Reliability, August 18,
Orlando
Reliability Issues with Lead-Free Soldering Processes, September 22,
Schaumburg
Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture,
ENIG), September 22, Schaumburg
Solder Joint Reliability: Parts 1 & 4, Oct. 9, Moscow, Russia
Solder Joint Reliability: Parts 1 & 4, Oct. 17, Timisoara, Rumania
Solder Joint Reliability: Parts 1 & 4, Oct. 22, Tallinn, Estonia
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|