TECHNET Archives

December 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Burtt, Nigel" <[log in to unmask]>
Date:
Tue, 1 Dec 1998 15:13:26 -0000
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, John Barton <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=ISO-8859-1
From:
John Barton <[log in to unmask]>
Parts/Attachments:
text/plain (68 lines)
Not exactly the UK but you can contact

Adrian Mulcahy,
NMRC,
Cork,
Ireland
Phone : +353-21-904226
Fax   : +353-21-270271
e-mail: [log in to unmask]

___________________________________________________________
John Barton AKA JohnnyB
NMRC, Lee Maltings,               Phone : +353-21-904088
Prospect Row,                     Fax   : +353-21-270271
Cork, Ireland.                    e-mail: [log in to unmask]
"Whenever I'm faced with a difficult problem, I always think to
myself 'How would MacGyver deal with this?'"
----------------------------------------------------------------------------
---


----------
> From: Burtt, Nigel <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] PCB micro-sectioning
> Date: 01 December 1998 12:03
>
> Would anyone care to recommend an independent PCB micro-sectioning
> service in the UK for some studies we are carrying out on plating
> failures in small via holes.
>
> > Nigel Burtt
> > Production Engineering Manager
> > D - European HQ
> > Email: [log in to unmask]
> > Tel: 01793 842132
> > Fax: 01793 842101
> >
> >
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2