TECHNET Archives

February 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Date:
Fri, 17 Feb 2012 20:31:02 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (67 lines)
Never done cpk.... but run chart.  If start to drift towards upper limit, you cry out wolf, so you would never see a dog come out of the line. 

Joyce Koo
Materials Researcher - Materials Interconnect Lab
Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Friday, February 17, 2012 3:22 PM
To: [log in to unmask]
Subject: Re: [TN] Correlation Factors for ROSE Testing & Cpk

Thanks to all who responded to this string. Realized it could strike a chord. 


To carry this a step further on a very related topic... 

Any of you guys ever try to run a Cpk on ROSE data sets?  Most of the times I've tried to over the years, the data sets have been non-normal, single tailed distributions, with highest counts near zero and then tailing off towards 10.06. (Similar to having only the right side half of a normal distribution curve).  They have defied data transformation to a normal distribution, hence can't really run a proper capability analysis (data of course must be normal for a Cpk).  

You could of course (at least within Minitab) try to run as a non-normal distribution and just report a PpK, however with such a high count near zero it's next to impossible to find a statistically supportable non-normal distribution. 

I would appreciate any related experiences and/or thoughts on this topic.  


Rich Kraszewski

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Thursday, February 16, 2012 2:00 PM
To: [log in to unmask]
Subject: [TN] Correlation Factors for ROSE Testing

While I realize that IPC specifically and the industry in general, does not support the use of ROSE correlation factors for the various testers, I have a need to see the official document that at one time quoted these specifically allowed factors.

I took a cursory look though all 230 pages of IPC TR 583 and didn't see that table. 

I seem to recall a military specification that had that table. Was it 454? 28809, 2000?

Does anyone recall?


Rich  Kraszewski / PLEXUS
 



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2