Hi Greg!
There has been very good advice given by many. I believe that the key is to keep the melt at just above freezing. So, it does not take so much time for the material removed to freeze back up again. Another matter, If there is a concern with metal contamination, use stainless steel shallow pans. They are readily available and do not cost too much.
Just my 2 cents.
Regards,
Ramon
TechNet:
We are going to drain and clean a wave solder pot in preparation for
conversion to lead-free solder.
We have not completely purged a wave solder pot in some time, and the
people in the know have moved on.
Does anyone have "best practices" recommendations for draining and handling
the solder (other than BE VERY CAREFUL ! ) ?
Greg Anderson
GE Fanuc Automation
Charlottesville, VA
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|