TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Kenneth Kirby <[log in to unmask]>
Date:
Thu, 7 Oct 1999 15:05:26 -0500
Content-type:
multipart/mixed; Boundary="0__=82qHSZjh1BdnHgqOkj0TGxR5sKdsyD9g1kQD25VNufEOWI2A7ALkgiNE"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Kenneth Kirby <[log in to unmask]>
Parts/Attachments:
text/plain (1707 bytes) , pic06352.pcx (2490 bytes)



Julie,
You must be soldering bare copper/OSP boards if your getting copper
contamination in your bath.  There is not much you can do about it but the
contamination will build up quicker in small solder pots as opposed to the
larger (1000 lbs +)pots.
If your not soldering copper boards then start looking for the person that
is throwing pennys into the bath. (Yes, I have seen this happen)  If you
have any doubt about the solder your using then you should have it analysed
by someone other than your vendor.

Ken Kirby




 (Embedded
 image moved   Julie Dixon <[log in to unmask]>
 to file:      10/07/99 01:59 PM
 pic06352.pcx)




To:   [log in to unmask]
cc:    (bcc: Kenneth Kirby/ElectrovertUS/Cookson)
Subject:  [TN] HASL-contaminated solder pot




TechNet,

We have sporadic problems with the copper level rising in our solder pot.
We
reduce the temp and dross each morning. Could you recommend a specific PM
program to keep our SnPb clean? We believe per the certicates of analyses
that
our supplier gives us good product. Any other reasons it might rise?

Thanks,
Green

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################




ATOM RSS1 RSS2