TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Kevin Glidden <[log in to unmask]>
Date:
Thu, 29 Nov 2007 09:01:19 -0500
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
R&D Assembly
MIME-Version:
1.0
Parts/Attachments:
text/plain (58 lines)
Without a nickel barrier the finish can dissolve completely into the solder
leaving the component bare. The defect condition is identified in the IPC
standards as leaching. This finish is common in applications when the
magnetic properties of nickel are unacceptable. A small amount of silver in
the paste, seems to widen the processing window.  

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden
Sent: Thursday, November 29, 2007 8:15 AM
To: [log in to unmask]
Subject: [TN] Palladium Silver Surface Finish

Hi everyone, 

 

An EE asked me about an SMT component he wants to use, but it is available
in only palladium-silver finish.  He was asking if that finish is acceptable
to use in our process (Sn63Pb37 alloy).  I have never used this finish
before.  Any caveats?  In case it matters, the component is an 1825 ceramic
cap.

 

Thanks in advance.

 

Kevin Glidden

Manufacturing Engineer

Luminescent Systems Inc.


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2