TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ed Popielarski <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ed Popielarski <[log in to unmask]>
Date:
Sun, 20 Jan 2008 07:08:30 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (99 lines)
Brian (and anyone else visiting the desert),

 

NEVER underestimate the power of flash flood. It's difficult to judge the
depth and fatalities are common! I personally watched a wall of water &
debris approx. 10-12 ft high come rushing down a canyon that my Cub Scout
Pack was exploring only an hour before (thanks to a park ranger for pointing
out the potential danger). 

 

http://www.youtube.com/watch?v=eqMEKA2BN7I

 

 

Regards,

 

Ed Popielarski

QTA Machine

17646 Fremont St.

Fountain Valley, Ca. 92708

Ph: 949-581-6601

 

  

Work is of two kinds: first, altering the position of matter at or near the
earth's surface relative to other matter; second, telling other people to do
so.

-Bertrand Russell (1872-1970)

http://www.youtube.com/watch?v=JYHJ1kZBMgU
<http://www.youtube.com/watch?v=JYHJ1kZBMgU&NR=1> &NR=1

http://www.youtube.com/watch?v=XlwB1uSTUmc
<http://www.youtube.com/watch?v=XlwB1uSTUmc&NR=1> &NR=1

http://www.youtube.com/watch?v=tqGzm841cAY

 

Date:    Sat, 19 Jan 2008 11:35:54 +0200

From:    Brian Ellis <[log in to unmask]>

Subject: Re: Solderability of Tin-Gold Intermetallic NTC

 

I had a Scotsman's "California moment". In April 1995, my wife and I were
doing some tourism. We reached Death Valley and started to explore it, by
car. Morning and early afternoon of one day we saw a lot, beautiful weather,
albeit slightly cooler than we expected. About 1400 h, we went up to see the
volcanic crater somewhere near the northern end. It suddenly clouded over
and, believe it or not, started to snow and, when I mean snow, it snowed
hard. Visibility was down to a few metres. And it was settling. We gingerly
made our way back down and after a couple of km, we were back down into
sheeting rain. Had to cross a couple of fairly minor flash floods before we
were back down into the valley. We then went to our motel at Stovepipe
Wells, passing the Devil's Cornfield, in beautiful sunshine, again.

 

Not the weather we expected in Death Valley!!!

 

Brian

 

 

 <http://www.nysdmv.com/media/gtsc_6_5_4_pm.mpg>  

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2